Request Quote
  1. Home
  2. Products
  3. Alloy Steel
  4. ASTM A213 T91 Alloy Steel Tubes

ASTM A213 T91 Alloy Steel Tubes

ASTM A213 T91 seamless 9Cr-1Mo-V creep resistant alloy steel tubes for supercritical boilers and HRSGs, supplied and exported by Riyaarth Overseas.

ASTM A213 T91 Alloy Steel Tubes by Riyaarth Overseas

ASTM A213 T91 tubes are seamless 9% chromium, 1% molybdenum, vanadium and niobium modified alloy steel tubes, often called modified 9Cr-1Mo. Grade T91 (UNS K90901) is a creep strength enhanced ferritic steel: its strength comes from a tempered martensite structure held stable by fine vanadium and niobium carbonitrides. That gives far higher creep strength than T22, so walls can be thinner and lighter.

T91 is widely used in supercritical boilers and heat recovery steam generators for superheater and reheater tubes. Because its properties depend on correct heat treatment, buyers look for tight chemistry, normalised and tempered condition and full records. Current editions of ASTM A213 list T91 as Type 1 and Type 2, the latter with tighter limits on several elements. Riyaarth Overseas supplies and exports ASTM A213 T91 tubes from established mill sources with complete documentation.

Key Features

High creep strength: Much higher allowable stresses than T22 at 550 – 600°C allow thinner walls and lower weight.

Oxidation resistance: About 9% chromium gives good resistance to steam oxidation in superheaters and reheaters.

Lower thermal stress: Thinner walls and a lower coefficient of expansion than austenitic steels reduce thermal fatigue during cycling.

Controlled heat treatment: Supplied normalised and tempered, which is essential for its long term properties.

Specifications

SpecificationDetails
StandardASTM A213 / ASME SA213
Grade / UNSGrade T91 / UNS K90901
Outside diameter range3.2 mm to 127 mm (1/8 in to 5 in), the range covered by ASTM A213
Wall thickness0.4 mm to 12.7 mm (0.015 in to 0.500 in), minimum or average wall
LengthRandom lengths, fixed lengths and U-bent tubes to drawing
TypeSeamless, hot finished or cold drawn
Heat treatmentNormalised at 1040 – 1080°C and tempered at 730 – 800°C
EndsPlain ends, square cut, deburred
Form / finishRound; black, pickled or varnished outside, as ordered
Test certificateEN 10204 3.1; 3.2 with third-party inspection (TPI) on request

Chemical Composition

ElementComposition (%)
Carbon (C)0.07 – 0.14
Manganese (Mn)0.30 – 0.60
Phosphorus (P)0.020 max
Sulphur (S)0.010 max
Silicon (Si)0.20 – 0.50
Chromium (Cr)8.0 – 9.5
Molybdenum (Mo)0.85 – 1.05
Nickel (Ni)0.40 max
Vanadium (V)0.18 – 0.25
Niobium (Nb)0.06 – 0.10
Nitrogen (N)0.030 – 0.070
Aluminium (Al)0.02 max
Titanium (Ti)0.01 max
Zirconium (Zr)0.01 max

Limits shown are for T91 Type 1. T91 Type 2 in current editions of ASTM A213 has tighter limits on several elements; state the type on the order.

Mechanical Properties

PropertyValue
Tensile strength585 MPa (85 ksi) min
Yield strength415 MPa (60 ksi) min
Elongation in 50 mm20% min
Hardness250 HBW max
Density7.77 g/cm³ (approx.)

Equivalent Grades

SystemEquivalent
UNSK90901
ASMESA213 T91
JIS G 3462STBA 28
EN 10216-2X10CrMoVNb9-1 (1.4903)

Testing and Inspection

Creep strength enhanced ferritic steels need tighter control than plain chrome-moly grades. Testing to ASTM A213 / A1016 and the order includes:

  • Hydrostatic or non-destructive electric test: on every length, with ultrasonic testing commonly specified for power plant use.
  • Tensile and hardness tests: to confirm strength and that hardness is within limits after normalising and tempering.
  • Flattening and flaring tests: to confirm ductility.
  • Positive material identification (PMI): to confirm Cr, Mo and the micro-alloying elements on every length.
  • Heat treatment records: normalising and tempering temperatures and times on the mill certificate.
  • Third-party and IBR inspection: available on request for boiler applications in India.

Why Choose Riyaarth Overseas

Riyaarth Overseas sources ASTM A213 T91 tubes from established boiler tube mills that control the normalise and temper cycle and the micro-alloying chemistry. We supply cut lengths with EN 10204 3.1 certificates, heat treatment records and PMI reports, and arrange 3.2 or IBR inspection on request. Send your sizes and type for a quick quote.

Applications

Supercritical power plantsUsed in final superheater and reheater sections of supercritical and ultra-supercritical boilers.
Heat recovery steam generatorsSpecified for high pressure superheater and reheater modules in combined cycle plants.
Steam headers and linksUsed for connecting tubes and small bore piping in hot steam circuits.
Refinery heatersSelected for heater coils where sulphur and high temperatures attack lower alloy steels.
Petrochemical plantsUsed in high temperature process heaters and exchangers.
Nuclear and solar thermalUsed in steam generators and receivers that need high temperature strength.

Frequently asked questions

What is the difference between T91 and T9?

T9 is a plain 9Cr-1Mo steel. T91 adds vanadium, niobium and nitrogen and is supplied normalised and tempered, which gives much higher creep strength.

Why does T91 need careful heat treatment?

Its strength comes from tempered martensite and fine carbonitrides. Wrong normalising, tempering or post-weld heat treatment temperatures can lower creep strength sharply, so controls and records matter.

What is T91 Type 2?

Type 2 is a variant added to ASTM A213 with tighter limits on certain elements and impurities, aimed at better long term creep performance. The order should state which type is needed.

What filler metal is used to weld T91?

Matching 9Cr-1Mo-V filler metals, such as ER90S-B9 or E9015-B9, are normally used, followed by post-weld heat treatment.