Stainless Steel 316Ti Pipes & Tubes
Stainless steel 316Ti pipes and tubes (UNS S31635, 1.4571) to ASTM A312 and EN 10216-5, titanium stabilised, supplied and exported by Riyaarth Overseas.

Stainless steel 316Ti (UNS S31635, EN 1.4571) is a titanium stabilised version of 316. Titanium combines with carbon and nitrogen, so chromium carbides do not form at grain boundaries when the steel is held between about 425 °C and 815 °C. This protects the material from intergranular corrosion after welding or during long service at those temperatures.
316Ti is widely specified in Europe, where 1.4571 tube to EN 10216-5 and EN 10217-7 is a common choice for chemical plants and heat exchangers. Riyaarth Overseas supplies and exports 316Ti seamless and welded pipes and tubes to ASTM and EN standards, with full mill certification.
Key Features
Titanium stabilised: Titanium of at least five times carbon plus nitrogen ties up carbon and prevents sensitisation in the weld zone.
Molybdenum bearing: With 2.00% to 3.00% Mo, it gives 316 level resistance to pitting and crevice corrosion.
Strength at temperature: Stabilisation allows good strength and resistance to intergranular attack at elevated temperature.
European standard grade: Matches the widely used 1.4571, making it easy to replace existing installations built to EN standards.
Specifications
| Parameter | Details |
|---|---|
| Standards | ASTM A312 / ASME SA312 (pipe), ASTM A213 / ASME SA213 (tube), EN 10216-5 (seamless), EN 10217-7 (welded) |
| Grade / UNS | TP316Ti (S31635), EN 1.4571 |
| Outside diameter range | Pipe: 1/8 in to 24 in NPS; tube: from 6 mm OD upward |
| Wall thickness / schedule | Schedule 5S to 80S and heavier on request; tube wall to order |
| Length | Single random, double random and cut lengths |
| Type | Seamless and welded |
| Ends | Plain end, bevelled end |
| Form / finish | Round; annealed and pickled |
| Test certificate | EN 10204 3.1 mill test certificate as standard; EN 10204 3.2 with third-party inspection on request |
Projects designed to European standards often call for 1.4571 to EN 10216-5 or EN 10217-7, while ASME projects call for TP316Ti to SA312. Tubes can be supplied with dual marking where the mill certifies both, which simplifies replacement work on existing plant.
Chemical Composition
Limits per ASTM A312 for UNS S31635. EN 1.4571 limits differ slightly.
| Element | Composition (%) |
|---|---|
| Carbon (C) | 0.08 max |
| Manganese (Mn) | 2.00 max |
| Phosphorus (P) | 0.045 max |
| Sulphur (S) | 0.030 max |
| Silicon (Si) | 0.75 max |
| Chromium (Cr) | 16.0 – 18.0 |
| Nickel (Ni) | 10.0 – 12.0 |
| Molybdenum (Mo) | 2.00 – 3.00 |
| Nitrogen (N) | 0.10 max |
| Titanium (Ti) | 5 × (C + N) min, 0.70 max |
Mechanical Properties
Room temperature minimums per ASTM A312 for UNS S31635. EN 10216-5 sets its own minimums for 1.4571, which should be used on EN projects.
| Property | Value |
|---|---|
| Tensile strength, min | 515 MPa (75 ksi) |
| Yield strength (0.2%), min | 205 MPa (30 ksi) |
| Elongation in 50 mm, min | 35% longitudinal, 25% transverse |
| Hardness | HBW 192 max / HRB 90 max (ASTM A213, A249, A269 tubes) |
| Density | approx. 8.0 g/cm³ |
Equivalent Grades
| System | Designation |
|---|---|
| UNS | S31635 |
| EN / Werkstoff | 1.4571 (X6CrNiMoTi17-12-2) |
| JIS | SUS316Ti |
| AISI | 316Ti |
Note that EN 1.4571 composition limits are not identical to ASTM S31635, so dual certification should be confirmed on the mill certificate.
Testing and Inspection
316Ti pipes and tubes are tested to the ordered ASTM or EN standard.
- Hydrostatic or eddy current test: Every length is pressure tested or checked by a non-destructive electric test.
- Intergranular corrosion test: ASTM A262 Practice E or EN ISO 3651-2 to confirm resistance after sensitising.
- Flattening and flaring tests: To confirm ductility.
- Positive material identification: Confirms the presence of titanium and molybdenum.
- Mechanical tests: Tensile, yield, elongation and hardness per lot.
- Third-party inspection: Available with EN 10204 3.2 certificates.
Certificates list titanium and carbon content so the stabilisation ratio can be checked, along with the heat treatment and the results of any corrosion test ordered.
Why Choose Riyaarth Overseas
Riyaarth Overseas supplies 316Ti pipes and tubes from European and Indian mill sources, with certificates to EN 10204 3.1 that show both ASTM and EN grade where the material is dual marked. We cut to length and pack securely for export. Send us your specification for a prompt offer.
Applications






Frequently asked questions
What is the difference between 316Ti and 316L?
Both are designed to avoid sensitisation. 316L does it by keeping carbon very low, while 316Ti adds titanium to tie up carbon. 316Ti keeps better strength at high temperature, while 316L is more common outside Europe.
Is 316Ti the same as 1.4571?
Yes, 1.4571 (X6CrNiMoTi17-12-2) is the European designation for titanium stabilised 316. The composition limits in EN and ASTM differ slightly, so check which standard the project requires.
Can 316L replace 316Ti?
In many wet corrosion services 316L is accepted as a substitute. For long service in the 425 °C to 815 °C range or where the design code names 1.4571, 316Ti should be kept.
Why is 316Ti hard to polish?
Titanium carbonitride particles in the steel can leave small marks on a mirror polished surface, so 316Ti is not usually chosen for decorative polished parts.