Stainless steel 904L pipes and tubes (UNS N08904, 1.4539) to ASTM B677, B673 and A312 for sulphuric acid and seawater duty, exported by Riyaarth Overseas.

Stainless Steel 904L Pipes & Tubes by Riyaarth Overseas

Stainless steel 904L (UNS N08904, EN 1.4539) is a high alloy, low carbon austenitic stainless steel with about 20% chromium, 25% nickel, 4.5% molybdenum and 1.5% copper. The copper addition gives good resistance to sulphuric acid, while the high molybdenum and nickel provide resistance to pitting, crevice corrosion and chloride stress corrosion cracking.

Seamless 904L pipe and tube are covered by ASTM B677, welded pipe by ASTM B673 and welded tube by ASTM B674, and the grade is also listed in ASTM A312. Riyaarth Overseas supplies and exports 904L pipes and tubes for acid plants, seawater cooling and chemical processing.

Key Features

Sulphuric acid resistance: Copper and high nickel give useful resistance across a wide range of sulphuric acid concentrations at moderate temperatures.

Pitting resistance: With about 4.5% molybdenum, 904L has a PREN of around 35, well above 316L.

Stress corrosion resistance: High nickel gives much better resistance to chloride stress corrosion cracking than standard austenitic grades.

Low carbon: Carbon of 0.020% max keeps the material resistant to intergranular corrosion after welding.

Specifications

ParameterDetails
StandardsASTM B677 / ASME SB677 (seamless pipe and tube), ASTM B673 / SB673 (welded pipe), ASTM B674 / SB674 (welded tube), ASTM A312, EN 10216-5
Grade / UNSUNS N08904, EN 1.4539
Outside diameter rangePipe: 1/8 in to 12 in NPS and larger in welded form; tube: from 6 mm OD upward
Wall thickness / scheduleSchedule 5S, 10S, 40S, 80S; tube wall to order
LengthSingle random, double random and cut lengths
TypeSeamless and welded
EndsPlain end, bevelled end
Form / finishRound; annealed and pickled
Test certificateEN 10204 3.1 mill test certificate as standard; EN 10204 3.2 with third-party inspection on request

Since 904L is covered by both ASTM A and ASTM B standards, check which one your project specification names, as the phosphorus and sulphur limits differ slightly. Matching fittings are available to ASTM B366 and flanges to ASTM B649 or A182.

Chemical Composition

Limits per ASTM A312 for UNS N08904, with the B677 limits shown where they differ.

ElementComposition (%)
Carbon (C)0.020 max
Manganese (Mn)2.00 max
Phosphorus (P)0.040 max (A312), 0.045 max (B677)
Sulphur (S)0.030 max (A312), 0.035 max (B677)
Silicon (Si)1.00 max
Chromium (Cr)19.0 – 23.0
Nickel (Ni)23.0 – 28.0
Molybdenum (Mo)4.0 – 5.0
Copper (Cu)1.00 – 2.00
Nitrogen (N)0.10 max

Mechanical Properties

Minimum values per ASTM A312 and B677 for solution annealed material. 904L is not hardenable by heat treatment; strength can only be raised by cold work.

PropertyValue
Tensile strength, min490 MPa (71 ksi)
Yield strength (0.2%), min215 MPa (31 ksi)
Elongation in 50 mm, min35%
Densityapprox. 8.0 g/cm³

Equivalent Grades

SystemDesignation
UNSN08904
EN / Werkstoff1.4539 (X1NiCrMoCu25-20-5)
JISSUS890L
Common name904L, Alloy 904L

Grades such as UNS N08925 and N08926 (6Mo grades) are higher alloyed alternatives and are not equivalents of 904L.

Testing and Inspection

904L pipes and tubes are tested to ASTM B677, B673, B674 or A312 as ordered.

  • Hydrostatic or eddy current test: On every length.
  • Positive material identification: Confirms nickel, molybdenum and copper levels.
  • Flattening and flaring tests: To confirm ductility.
  • Intergranular corrosion test: ASTM A262 Practice C or E as specified by the buyer.
  • Pitting corrosion test: ASTM G48 on request for critical chloride service.
  • Third-party inspection: Witness inspection with EN 10204 3.2 certification.

Certificates list the full chemistry including copper and molybdenum, the solution annealing temperature and all test results, and each length is marked with UNS number, size and heat number.

Why Choose Riyaarth Overseas

Riyaarth Overseas sources 904L pipes and tubes from specialist mills and supplies them with EN 10204 3.1 certificates, heat traceability and PMI on request. We cut to length and pack for export, and can include 904L fittings and flanges in the same order. Send your enquiry for a fast quote.

Applications

Sulphuric acid plantsAcid coolers, transfer lines and distribution piping.
Phosphoric acid productionEvaporator tubes and lines in wet process phosphoric acid plants.
Seawater coolingCondenser and cooler tubes where 316L would pit.
Pulp and paperBleach plant equipment exposed to chlorides and acids.
Pharmaceutical and chemicalReactors and process lines handling acidic, chloride bearing media.
Oil and gasHeat exchanger tubes and process piping in sour or brine service.

Frequently asked questions

Is 904L a stainless steel or a nickel alloy?

904L is classed as a high alloy austenitic stainless steel. Because its nickel content is over 23%, it carries a UNS N number (N08904) and is covered by ASTM B standards as well as ASTM A312.

How does 904L compare with 316L?

904L has much higher nickel and molybdenum plus copper, so it resists sulphuric acid, pitting and chloride stress corrosion cracking far better than 316L, at a higher cost.

What is the EN equivalent of 904L?

The European equivalent is 1.4539 (X1NiCrMoCu25-20-5).

Which standard covers seamless 904L tube?

ASTM B677 / ASME SB677 covers seamless UNS N08904 pipe and tube.