ASTM A335 P9 Alloy Steel Pipes

ASTM A335 P9 seamless 9Cr-1Mo alloy steel pipes for refinery heaters and high temperature sulphur service, supplied and exported by Riyaarth Overseas.

ASTM A335 P9 Alloy Steel Pipes by Riyaarth Overseas

ASTM A335 P9 pipes are seamless ferritic alloy steel pipes with about 9% chromium and 1% molybdenum. ASTM A335, and its boiler code version ASME SA335, covers seamless alloy steel pipe for high temperature service, and grade P9 (UNS K90941) is the plain 9Cr-1Mo grade, without the vanadium and niobium additions of P91.

Refiners specify P9 mainly for its resistance to high temperature sulphidation and oxidation, for example in fired heater coils and furnace piping handling sulphur-bearing crude. Its higher chromium resists sulphur attack far better than P5 or P22. Riyaarth Overseas supplies and exports ASTM A335 P9 pipes from established mill sources, in schedule sizes with bevelled ends, with EN 10204 3.1 certificates.

Key Features

Sulphidation resistance: About 9% chromium gives strong resistance to high temperature sulphur corrosion in refinery heaters.

Oxidation resistance: Suitable for hot flue gas and steam environments where lower chromium steels scale quickly.

Silicon added: 0.25 – 1.00% silicon helps oxidation resistance at elevated temperature.

Air hardening: P9 hardens on air cooling, so welding needs preheat and post-weld heat treatment.

Specifications

SpecificationDetails
StandardASTM A335 / ASME SA335
Grade / UNSGrade P9 / UNS K90941
Outside diameter rangeNPS 1/8 upwards, dimensions to ASME B36.10M
Wall thickness / scheduleSCH 10 to SCH 160, STD, XS, XXS, or specified wall
LengthSingle random, double random and cut lengths
TypeSeamless, hot finished or cold drawn
Heat treatmentFull or isothermal anneal, or normalise and temper
EndsPlain ends, bevelled ends to ASME B16.25
Form / finishRound; black, varnished or pickled, as ordered
Test certificateEN 10204 3.1; 3.2 with third-party inspection (TPI) on request

Chemical Composition

ElementComposition (%)
Carbon (C)0.15 max
Manganese (Mn)0.30 – 0.60
Phosphorus (P)0.025 max
Sulphur (S)0.025 max
Silicon (Si)0.25 – 1.00
Chromium (Cr)8.00 – 10.00
Molybdenum (Mo)0.90 – 1.10

Mechanical Properties

PropertyValue
Tensile strength415 MPa (60 ksi) min
Yield strength205 MPa (30 ksi) min
Elongation, longitudinal30% min
Elongation, transverse20% min
Density7.75 g/cm³ (approx.)

ASTM A335 does not set a hardness limit for P9 in the base specification; a maximum hardness can be added on the order.

Equivalent Grades

SystemEquivalent
UNSK90941
ASMESA335 P9
JIS G 3458STPA 26
EN 10216-2X11CrMo9-1 (1.7386)

Testing and Inspection

Every lot is tested to ASTM A335 / A999 and the general requirements it references, plus any supplementary requirements on the order:

  • Hydrostatic or non-destructive electric test: each tube or pipe is hydro tested or checked by eddy current or ultrasonic testing.
  • Tensile test: tensile strength, yield strength and elongation.
  • Flattening and flaring tests: to confirm ductility (flattening or bend test for pipe).
  • Hardness test: where the grade or order sets a hardness limit.
  • Positive material identification (PMI): to confirm chromium and molybdenum on every length when ordered.
  • Dimensional and visual inspection: outside diameter, wall, length and surface.
  • Third-party inspection: by agencies such as TUV, BV, SGS or Lloyd's Register on request.

Why Choose Riyaarth Overseas

Riyaarth Overseas sources ASTM A335 P9 pipes from established seamless pipe mills and supplies them in standard schedules, cut lengths and bevelled ends. Pipes come with EN 10204 3.1 mill test certificates and PMI reports on request, and are packed for export with end caps and bundling. Send your sizes and schedules for a prompt quote.

Applications

Refinery fired heatersUsed for radiant and convection coils and crossover piping in crude and vacuum heaters.
Coker and visbreaker unitsSelected for heater tubes handling hot, sulphur-bearing residue.
HydroprocessingUsed in high temperature lines where sulphur and hydrogen are present.
Petrochemical furnacesInstalled in furnace piping exposed to high temperature process gas.
Power plant pipingUsed in some steam and boiler piping in older designs.
Heat exchangersUsed for high temperature exchanger piping in sulphur service.

Frequently asked questions

What is the difference between P9 and P91?

P9 is plain 9Cr-1Mo steel. P91 adds vanadium, niobium and nitrogen and is normalised and tempered, which gives much higher creep strength. P9 is mainly chosen for sulphidation resistance in refinery service.

Why is P9 used in refinery heaters?

Its 8 – 10% chromium resists high temperature sulphidation from sulphur-bearing crudes much better than lower chromium steels such as P5 or P22.

Do P9 pipes need preheat for welding?

Yes. P9 hardens on cooling, so preheat, controlled interpass temperature and post-weld heat treatment are normally required.

What is the tube equivalent of P9?

ASTM A213 T9 tubes share the same UNS number, K90941, and chemistry.