Incoloy 825 (UNS N08825) seamless and welded pipes and tubes to ASTM B423, B163 and B705, stocked and exported by Riyaarth Overseas, Mumbai.

Incoloy 825 Pipes & Tubes by Riyaarth Overseas

Incoloy 825 is an iron-nickel-chromium alloy with additions of molybdenum, copper and titanium, designated UNS N08825 and Werkstoff 2.4858. The nickel content of 38 to 46 percent gives strong resistance to chloride stress corrosion cracking, while molybdenum and copper give it resistance to reducing acids such as sulphuric and phosphoric acid. Titanium stabilises the carbon, which protects the alloy against intergranular attack after welding.

Pipes and tubes in this grade are made to ASTM B423 (seamless pipe and tube), ASTM B163 (seamless condenser and heat exchanger tubes), ASTM B705 (welded pipe) and ASTM B704 (welded tube), with the matching ASME SB designations for code work. Riyaarth Overseas supplies and exports Incoloy 825 pipes and tubes from stock and from approved mill sources, cut to length and documented for oil and gas, chemical, pollution control and marine projects.

Key Features

Resistance to sulphuric and phosphoric acid: The combination of molybdenum and copper gives Incoloy 825 good service life in sulphuric acid pickling lines and phosphoric acid plants, where standard austenitic stainless steels corrode quickly.

Chloride stress corrosion cracking resistance: With nickel above 38 percent, the alloy is far less prone to chloride stress corrosion cracking than 300-series stainless steel, which makes it a common choice for sour gas and seawater-cooled duties.

Titanium stabilised: Titanium ties up carbon as titanium carbide, so the alloy resists sensitisation and intergranular corrosion in the weld heat affected zone without post-weld heat treatment.

Good fabricability: Incoloy 825 can be bent, expanded into tube sheets and welded with matching or overmatching nickel alloy filler metals using standard TIG and MIG procedures.

Specifications

ParameterDetails
StandardsASTM B423 / ASME SB423, ASTM B163 / ASME SB163, ASTM B705 / ASME SB705, ASTM B704 / ASME SB704
Grade / UNSIncoloy 825, UNS N08825, W.Nr. 2.4858
Outside diameter rangeSeamless tube from 6.35 mm (1/4 in) OD; pipe NPS 1/8 in to 8 in seamless, larger sizes in welded form
Wall thickness / scheduleSCH 5S, 10S, 40S, 80S, 160, XXS; tube walls in BWG or mm as ordered
LengthSingle random, double random and cut lengths
TypeSeamless, welded, welded and drawn
EndsPlain ends, bevelled ends, threaded ends on request
Form / finishRound, U-bent heat exchanger tube, coiled tube; annealed and pickled, bright annealed
Test certificateEN 10204 3.1 mill test certificate as standard; EN 10204 3.2 with third-party inspection on request

Chemical Composition

ElementComposition (%)
Nickel (Ni)38.0 – 46.0
Iron (Fe)22.0 min
Chromium (Cr)19.5 – 23.5
Molybdenum (Mo)2.5 – 3.5
Copper (Cu)1.5 – 3.0
Titanium (Ti)0.6 – 1.2
Carbon (C)0.05 max
Manganese (Mn)1.0 max
Silicon (Si)0.5 max
Sulphur (S)0.03 max
Aluminium (Al)0.2 max

Mechanical Properties

PropertyValue
Tensile strength (annealed)85 ksi (586 MPa) min
Yield strength, 0.2% offset35 ksi (241 MPa) min
Elongation in 2 in (50 mm)30% min
Density8.14 g/cm³
Melting range1370 – 1400 °C

Minimum values are for the annealed condition as required by ASTM B423 and B163.

Equivalent Grades

StandardDesignation
UNSN08825
Werkstoff Nr.2.4858
ENNiCr21Mo
JISNCF 825
Common namesIncoloy 825, Alloy 825

Testing and Inspection

Each lot of Incoloy 825 pipe and tube is tested to the requirements of the ordered ASTM or ASME specification before dispatch. Typical checks include:

  • Hydrostatic or non-destructive electric test: Every length is hydrotested or checked by eddy current as the standard requires.
  • Flattening and flaring tests: To confirm ductility of the tube wall.
  • Positive material identification (PMI): To confirm nickel, chromium, molybdenum and copper on each piece.
  • Intergranular corrosion test: ASTM G28 or other IGC testing on request for critical acid service.
  • Dimensional and visual inspection: OD, wall thickness, length and surface checked against the order.
  • Third-party inspection: Witness inspection by agencies such as TUV, BV, SGS or Lloyds on request.

Why Choose Riyaarth Overseas

Riyaarth Overseas keeps Incoloy 825 pipes and tubes in ready stock and sources further sizes from established nickel alloy mills, so standard and project sizes can be supplied in single random, double random or cut lengths. Every shipment carries EN 10204 3.1 mill test certificates with heat numbers marked on each length.

Material is packed for export in wooden boxes or bundles with end caps, and we send quotations quickly against your drawings, data sheets or bill of materials.

Applications

Oil and gasDownhole tubing, flowlines and process piping for sour gas wells containing hydrogen sulphide and chlorides.
Sulphuric acid plantsHeating coils, heat exchanger tubes and transfer piping in acid production and steel pickling lines.
Pollution controlFlue gas desulphurisation scrubbers and ducting where condensed acids and chlorides attack lower alloys.
Marine and seawater coolingSeawater-cooled heat exchanger tubing and piping on offshore platforms and ships.
Chemical processingPhosphoric acid evaporators and mixed acid service where molybdenum and copper give added protection.
Nuclear fuel reprocessingDissolver and evaporator equipment exposed to nitric acid and spent fuel solutions.

Frequently asked questions

Which ASTM standard covers Incoloy 825 seamless pipe?

ASTM B423 (ASME SB423) covers seamless Incoloy 825 pipe and tube. Condenser and heat exchanger tubes are usually ordered to ASTM B163, and welded pipe to ASTM B705.

How is Incoloy 825 different from 316L stainless steel?

Incoloy 825 contains far more nickel, plus copper and titanium, which gives much better resistance to chloride stress corrosion cracking and to sulphuric and phosphoric acids than 316L.

Does Incoloy 825 need heat treatment after welding?

Normally no. The titanium stabilisation prevents chromium carbide precipitation, so welded joints keep their resistance to intergranular corrosion in the as-welded condition.

Can you supply U-bent Incoloy 825 heat exchanger tubes?

Yes. Riyaarth Overseas supplies ASTM B163 Incoloy 825 tubes in straight lengths and U-bent form to your bend schedule, with test certificates for each heat.