ASTM A210 / ASME SA210 Grade A-1 and Grade C seamless medium carbon steel boiler and superheater tubes, supplied and exported by Riyaarth Overseas, Mumbai.

ASTM A210 / SA210 Tubes by Riyaarth Overseas

ASTM A210 covers seamless medium carbon steel tubes for boiler tubes, boiler flues, superheater flues, safe ends, arch and stay tubes, and superheater tubes. ASME SA-210 is the code version. The specification has two grades: Grade A-1 and Grade C. Grade C has higher carbon and manganese, giving higher strength than Grade A-1, and both are stronger than the low carbon A192 tube.

The specification covers tubes from 1/2 in. to 5 in. (12.7 to 127 mm) outside diameter, with minimum wall thickness from 0.035 in. to 0.500 in. (0.9 to 12.7 mm). Tubes are made seamless, hot finished or cold drawn, and cold drawn tubes are heat treated after the final draw. The higher strength of A210 lets designers use thinner walls than A192 for the same pressure.

Riyaarth Overseas supplies and exports ASTM A210 / SA210 tubes in Grade A-1 and Grade C from mill sources for boiler makers and power and process plants.

Key Features

Two strength levels: Grade A-1 gives 415 MPa minimum tensile strength and Grade C gives 485 MPa, so the designer can match strength to duty.

Thinner walls for the same pressure: Higher allowable stresses than A192 reduce tube weight in boiler and superheater circuits.

Killed steel: A minimum silicon of 0.10% gives a killed, sound steel for pressure parts.

Hardness controlled: Maximum hardness limits for each grade keep the tube suitable for bending and expanding.

Specifications

ItemDetails
StandardASTM A210 / ASME SA-210
GradesGrade A-1, Grade C
Outside diameter1/2 in. to 5 in. (12.7 to 127 mm)
Wall thickness0.035 in. to 0.500 in. (0.9 to 12.7 mm) minimum wall
LengthFixed and random lengths
TypeSeamless, hot finished or cold drawn
EndsPlain ends, bevelled ends
Form / finishHot finished, or heat treated after cold drawing; varnished or oiled
Test certificateEN 10204 3.1 standard; EN 10204 3.2 with third-party witness on request

Chemical Composition

ElementGrade A-1Grade C
Carbon (C)0.27 max0.35 max
Manganese (Mn)0.93 max0.29 – 1.06
Phosphorus (P)0.035 max0.035 max
Sulphur (S)0.035 max0.035 max
Silicon (Si)0.10 min0.10 min

Mechanical Properties

PropertyGrade A-1Grade C
Tensile strength, min60 ksi (415 MPa)70 ksi (485 MPa)
Yield strength, min37 ksi (255 MPa)40 ksi (275 MPa)
Elongation in 2 in., min30%30%
Hardness, max79 HRB (143 HBW)89 HRB (179 HBW)

Equivalent Grades

Approximate equivalents for comparison only. Check limits before substitution.

A210 gradeComparable grades
Grade A-1EN 10216-2 P235GH; JIS G3461 STB 410
Grade CEN 10216-2 P265GH; JIS G3461 STB 510

Testing and Inspection

Testing follows ASTM A210 and the general requirements of ASTM A450.

  • Hydrostatic or electric test: Each tube is hydrostatically tested or passed through a non-destructive electric test.
  • Tensile test: Tensile and yield strength checked per lot.
  • Flattening and flaring: Flattening and flaring tests on each lot.
  • Hardness test: Rockwell or Brinell hardness checked against the grade limit.
  • Visual and dimensional: Checks on outside diameter, minimum wall and length.
  • Third-party inspection: Witness inspection, including IBR inspection for Indian boiler projects when ordered.

When ordering, state the grade (A-1 or C), outside diameter, minimum wall, length and quantity, and whether hot finished or cold drawn tubes are acceptable. Grade C is often chosen where a boiler maker wants to reduce tube weight, while Grade A-1 is common where tubes will be heavily formed. Superheater sections above the code limit for carbon steel need alloy steel tubes instead.

Why Choose Riyaarth Overseas

Riyaarth Overseas supplies ASTM A210 Grade A-1 and Grade C tubes from stock and mill sources, with cut lengths and end bevelling on request. Each order is shipped with EN 10204 3.1 mill test certificates and heat-wise traceability, and tubes are bundled and capped for export. Send your requirement for a quick quotation.

Applications

Boiler tubesUsed for waterwall, riser and generating tubes where higher strength than A192 is useful.
Superheater tubesUsed in superheater sections within the code temperature limits for carbon steel.
Boiler fluesUsed for boiler and superheater flues.
Stay and arch tubesUsed for arch tubes, stay tubes and safe ends in boiler construction.
Heat recovery steam generatorsUsed in HRSG evaporator and economiser tubes.
Process heat exchangersUsed in high pressure exchangers where carbon steel is acceptable and higher strength is needed.

Frequently asked questions

What is the difference between A210 Grade A-1 and Grade C?

Grade C has higher carbon and manganese limits and a higher minimum tensile strength of 485 MPa, against 415 MPa for Grade A-1.

How does A210 compare with A192?

A210 is a medium carbon steel with higher strength than the low carbon A192, so A210 tubes can use thinner walls at the same pressure.

What size range does A210 cover?

Outside diameters from 1/2 in. to 5 in. (12.7 to 127 mm), with minimum walls from 0.035 in. to 0.500 in.

Is A210 Grade C the same as SA210 Grade C?

Yes. ASME SA-210 adopts ASTM A210, and tubes are normally dual-marked.