ASTM A214 / SA214 Tubes
ASTM A214 / ASME SA214 electric resistance welded carbon steel tubes for heat exchangers and condensers, up to 3 in. OD, exported by Riyaarth Overseas.

ASTM A214 covers electric resistance welded (ERW) carbon steel tubes for heat exchangers, condensers and similar heat transfer equipment. ASME SA-214 is the code version. It is the welded counterpart of ASTM A179 and covers tubes up to 3 in. (76.2 mm) outside diameter.
A214 tubes are made from flat-rolled steel formed into a tube and welded by electric resistance without filler metal. After welding, tubes are heat treated at 1650 °F (900 °C) or higher and cooled in air or in the cooling chamber of a controlled atmosphere furnace; cold drawn tubes are heat treated after the final draw at 1200 °F (650 °C) or higher. Unlike most tube specifications, A214 sets a hardness limit but no tensile requirement, because the tube is mainly judged on its ability to be expanded and its weld integrity.
Riyaarth Overseas supplies and exports ASTM A214 / SA214 tubes for exchanger fabricators who need an economical welded alternative to seamless A179.
Key Features
Economical welded tube: ERW manufacture from strip costs less than seamless tube and gives uniform wall thickness.
Heat treated after welding: Normalising-type heat treatment after welding gives the weld zone properties close to the parent metal.
Expansion tested: Flattening, reverse flattening, flaring and flange tests confirm the weld and the tube can be expanded into tubesheets.
Soft tube: A hardness limit of 72 HRB keeps the tube suitable for rolling into tubesheets.
Specifications
| Item | Details |
|---|---|
| Standard | ASTM A214 / ASME SA-214 |
| Material | Low carbon steel |
| Outside diameter | Up to 3 in. (76.2 mm) |
| Wall thickness | Minimum or average wall as ordered (BWG gauges common) |
| Length | Fixed lengths to drawing; U-bends on request |
| Type | Electric resistance welded (ERW) |
| Ends | Plain ends, deburred |
| Form / finish | Heat treated at 900 °C (1650 °F) or higher after welding; oiled or varnished |
| Test certificate | EN 10204 3.1 standard; EN 10204 3.2 with third-party witness on request |
Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | 0.18 max |
| Manganese (Mn) | 0.27 – 0.63 |
| Phosphorus (P) | 0.035 max |
| Sulphur (S) | 0.035 max |
Mechanical Properties
| Property | Value |
|---|---|
| Hardness | 72 HRB max |
| Tensile and yield strength | Not specified by ASTM A214 |
| Mechanical tests required | Flattening, reverse flattening, flaring and flange tests |
Equivalent Grades
Approximate equivalents for comparison only. Check limits before substitution.
| Standard | Comparable grade |
|---|---|
| EN 10217-1 | P195TR1 / P195TR2 (welded) |
| JIS G3461 | STB 340 (ERW) |
Testing and Inspection
Testing follows ASTM A214 and the general requirements of ASTM A450.
- Hydrostatic or electric test: Each tube is hydrostatically tested or passed through a non-destructive electric test.
- Flattening test: Flattening test on each lot.
- Reverse flattening test: Reverse flattening test to check the weld.
- Flaring and flange tests: Flaring and flange tests to confirm the tube can be expanded and flanged.
- Hardness test: Rockwell hardness checked against the 72 HRB limit.
- Third-party inspection: Witness inspection by a nominated agency on request.
When ordering A214 tubes, state the outside diameter, minimum or average wall, length, quantity and any U-bend details. Because A214 has no tensile requirement, designers who need guaranteed strength values for pressure calculations should check the allowable stress values in the applicable code, or consider seamless A179 tubes where the specification or end user requires seamless construction. A214 tubes are used where the process fluids are compatible with plain carbon steel.
Why Choose Riyaarth Overseas
Riyaarth Overseas supplies ASTM A214 tubes from established ERW tube mills in exchanger lengths and U-bends. Every order ships with EN 10204 3.1 mill test certificates and is bundled with end caps in export packing. Send your tube sheet list for a fast quotation.
Applications






Frequently asked questions
What is the difference between ASTM A214 and A179?
A214 tubes are electric resistance welded, while A179 tubes are seamless and cold drawn. Both are low carbon exchanger tubes with a 72 HRB hardness limit.
Does ASTM A214 specify tensile strength?
No. A214 sets a maximum hardness of 72 HRB and requires flattening, reverse flattening, flaring and flange tests, but it has no tensile or yield requirement.
What size range does A214 cover?
The specification covers tubes up to 3 in. (76.2 mm) outside diameter.
Are A214 tubes heat treated?
Yes. After welding, tubes are heat treated at 900 °C (1650 °F) or higher, and cold drawn tubes are heat treated after the final draw.