ASTM A334 Carbon & Alloy Steel Tubes
ASTM A334 carbon and alloy steel tubes for low temperature service, Grades 1, 3 and 6, seamless and welded, impact tested, from Riyaarth Overseas, Mumbai.

ASTM A334 covers seamless and welded carbon and alloy steel tubes for low temperature service. It is the tubing counterpart of ASTM A333: where A333 is ordered by pipe size and schedule, A334 is ordered by outside diameter and wall thickness and is used for heat exchanger, condenser and instrument tubing in cold service. ASME SA-334 is the code version.
The specification includes several grades. Grade 1 and Grade 6 are carbon-manganese steels impact tested at -45 °C, and Grade 3 is a 3.5% nickel alloy steel impact tested at -100 °C for colder duty. Tubes are normalised or given another heat treatment that secures the required impact properties.
Riyaarth Overseas supplies and exports ASTM A334 tubes, most often Grade 6, from mill sources for exchanger builders, refrigeration contractors and plant maintenance teams.
Key Features
Grades for different temperatures: Grade 1 and Grade 6 suit service down to about -45 °C, while nickel-bearing Grade 3 is impact tested at -100 °C.
Impact tested tubing: Charpy tests on every heat confirm toughness, which ordinary boiler tube specifications do not require.
Seamless or welded: Both constructions are allowed, so buyers can choose welded tube for economy or seamless for heavier duty.
Hardness limits for expansion: Maximum hardness values help ensure tubes can be rolled into tubesheets without cracking.
Specifications
| Item | Details |
|---|---|
| Standard | ASTM A334 / ASME SA-334 |
| Grades | Grade 1, Grade 6 (carbon steel); Grade 3 (3.5% nickel); other listed grades on request |
| Outside diameter | Tube sizes to the order, subject to mill availability |
| Wall thickness | Average or minimum wall as ordered |
| Length | Fixed lengths, random lengths and U-bend lengths for exchanger work |
| Type | Seamless or welded |
| Ends | Plain ends |
| Form / finish | Normalised or otherwise heat treated as the standard allows |
| Test certificate | EN 10204 3.1 standard; EN 10204 3.2 with third-party witness on request |
Chemical Composition
| Element | Grade 1 | Grade 6 | Grade 3 |
|---|---|---|---|
| Carbon (C) | 0.30 max | 0.30 max | 0.19 max |
| Manganese (Mn) | 0.40 – 1.06 | 0.29 – 1.06 | 0.31 – 0.64 |
| Phosphorus (P) | 0.025 max | 0.025 max | 0.025 max |
| Sulphur (S) | 0.025 max | 0.025 max | 0.025 max |
| Silicon (Si) | … | 0.10 min | 0.18 – 0.37 |
| Nickel (Ni) | … | … | 3.18 – 3.82 |
Mechanical Properties
| Property | Grade 1 | Grade 6 | Grade 3 |
|---|---|---|---|
| Tensile strength, min | 55 ksi (380 MPa) | 60 ksi (415 MPa) | 65 ksi (450 MPa) |
| Yield strength, min | 30 ksi (205 MPa) | 35 ksi (240 MPa) | 35 ksi (240 MPa) |
| Hardness, max | 85 HRB (163 HBW) | 90 HRB (190 HBW) | 90 HRB (190 HBW) |
| Impact test temperature | -45 °C (-50 °F) | -45 °C (-50 °F) | -100 °C (-150 °F) |
Equivalent Grades
There is no exact foreign equivalent for ASTM A334 because impact test temperatures and acceptance values differ between standards. For low temperature tubes in European projects, EN 10216-4 (seamless) and EN 10217-6 (welded) grades such as P265NL are the usual alternatives, and 3.5% nickel steels are covered as 12Ni14 in EN 10216-4.
Testing and Inspection
Testing follows ASTM A334 and the general requirements of ASTM A1016.
- Charpy impact test: V-notch impact test at the grade test temperature on each heat.
- Hydrostatic or electric test: Each tube is hydrostatically tested or passed through a non-destructive electric test.
- Flattening and flaring: Flattening and flaring tests on seamless tube; flange and reverse flattening tests on welded tube.
- Hardness test: Rockwell or Brinell hardness on samples from each lot.
- Tensile test: Tensile and yield checked per lot.
- Third-party inspection: Witness inspection by a nominated agency on request.
Why Choose Riyaarth Overseas
Riyaarth Overseas supplies ASTM A334 tubes from ready stock and established mill sources, and can arrange cut lengths, bevelling and end protection to suit your project. Every shipment carries EN 10204 3.1 mill test certificates with full heat traceability, and material is bundled and marked for export. Send your size list for a fast quotation.
Applications






Frequently asked questions
What is the difference between ASTM A333 and A334?
A333 covers pipe ordered by nominal pipe size and schedule. A334 covers tubes ordered by outside diameter and wall thickness. Both are for low temperature service and share similar grades.
Which A334 grade is most common?
Grade 6 is the most commonly ordered grade for carbon steel low temperature tubing.
When is A334 Grade 3 used?
Grade 3 contains about 3.5% nickel and is impact tested at -100 °C, so it is used where Grade 6 is not tough enough.
Can A334 tubes be supplied as U-bends?
Yes. U-bend tubes can be arranged through the mill for heat exchanger orders, with stress relief of the bend area where specified.